The Creep testing machine is designed for Analyzing the characteristics of material against constant force & variable temperature.
The machine comprises of a lever assembly with dead weights, Tensile force application arrangement and furnace for heating of specimen.
DIGITAL CREEP TESTING MACHINE For Tensile Creep with high temperature range up to 1000 degree C for creep testing of various types of materials such as metal, S.Steel, aluminium, copper and other prescribed metals. The unit consisting of Frame comprising of Lever Arm– 1:10 ratio, Pull Rods, Gear Arrangement for moving Pull rod up or down for fixing the Specimen, Loading arrangement along with Standard loads of 10 Kg each, 3 Zone Furnace for 1000° C along with Temperature Controller, Thyristor Drive, LVDT for measuring Creep data etc.1.
Lever Arm, Frame, Loading Pan2.
Standard Weigh Pads of 10 kgs each3.
Motor, Motor Drive along with gear box4.
Specimen Holder5.
Extension Meter along with signal conditioner 6.
PC add on card with computer7.
Data Acquisition system and software8.
3 Zone cylindrical furnace – Temp. 1000 Degree C9.
Controller and heating Drive and cables and co
Technical specifications of Digital Creep Testing Machine –
Loading Arrangement
: Manual by dead weight
Specimen holding arrangement
: Made out of numonic alloy
Heating arrangement
: Cylindrical furnace 4 KW
Temp. Range
: Ambient to 1000
Degree Temp. controller
: PID
Temp. accuracy
: +/- 1 degree C
Temp. sensor
: K type thermocouple
Deflection sensor
: LVDT
Data Processing
: PC based data Acquisition system
Data output
: Deflection Vs Time
Sampling Interval
: User selectable in steps
Click On PDF File for complete details

RELATED PRODUCTS
 
X

Invalid Input
Please enter Mobile Number
Invalid Email ID
Invalid Email ID
Your Contact Information
Convenient
Competitive Quotes
Choice of Suppliers
Payment Protection
 
sending enquiry ....

unable to instantiate your call right now. please try after some time.

close

©Copyright HelloTrade.com