Gloss Varnish

Next Product »
FOB Price : Get Price

SUBSTRATES
Paper covered with PET/BOPP film, rigid PVC, ABS, PP.
END USES
General merchandise and publishing materials, such as food packaging, cosmetic, posters etc.
PRODUCT INFORMATION
Have good adhesion, flexibility, glossiness and flow capability to most of the matt paper and some of the gloss paper.
Items
Description
glossiness
Yellow changing resistance
Water resistance
Alkali resistance
Solvent resistance
flexibility
adhesion
UVH-gloss varnish
87-89
adjustable
Grade 5
Grade 4
Grade 3
Excellent
Acceptable
TECHNICAL PARAMETER
Items
Description
Appearance
Viscosity/25
Solidification Speed
Solidification Power
Resin
UVH-gloss varnish
Milky liquid
340-420
15-25m/min
120mj/cO
98%
APPLICATION INFORMATION
MESH
Monofilament mesh, 120-152T, tensility 13-15 N/cO
SQUEEGEE
65-75 durometer solvent resistance blade, such as PU
COVERAGE
Approx. 35-40O/kg under 140T mesh
CURE
By Ultra Violet curing machine, use 2 high/medium voltage mercury-vapor lamp at least 5KW to ensure sufficient UV power for curing.
Additives
Use UVH-1 thinner to reduce viscosity of the varnish, UVH cure promoter to improve cure speed.
CLEAN UP
Use organic solvent to clean the stencil, do not print until it is totally volatilized.
NOTE
1 As the UVH-Matte varnish has excellent flexibility, it may cause the phenomena of sticky and bad flow ability. To solve the problem, printer should churn up the varnish even and ensure good ventilation for the curing machine, take note to reduce the temperature of the paper, avoid stacking together to cause conglutination. Recommend to refrigerate by fan and place separately.
2 Take note of protection as some component of the varnish may be harmful to our skin. For skin contact, wash thoroughly with soap and water. For aye contact, flush thoroughly with waterand then send to hospital. Change the cloth if it is adhered with varnish.
3 Cleanness and treatment on the surface of the substrate is important factors to adhesion, it has good adhesion to substrates when the surface tensility is over 38 dynemake sure the tensility meets the printing requirement before usage.

RELATED PRODUCTS
 
X

Invalid Input
Please enter Mobile Number
Invalid Email ID
Invalid Email ID
Your Contact Information
Convenient
Competitive Quotes
Choice of Suppliers
Payment Protection
 
sending enquiry ....

unable to instantiate your call right now. please try after some time.

close

©Copyright HelloTrade.com